1: grass-roots treatment, should all clean up the walls of the various dirt, and water wet one day in advance. If the grass-roots for the new wall, when the cement mortar Qicheng dry, it should be row of brick, elastic line, towel wall tiles.

2: tile paste must be soaked in water for more than 2 hours before the brick body is not bubbling prevail, remove the dry stand.

3: pavement encountered in the pipeline, lighting switches, bathroom equipment, such as support, etc., must be cut with the whole brick sets, prohibited with non-brick together patch paste.

Floor tile laying Note:

1: tiles in the use of water for half a day before the brick body is not bubbling prevail.

2: kitchen, bathroom should have water gradient, no water, water does not turn back. Construction of the original waterproof layer, to be waterproof treatment, water 12 hours without leakage test.

3: After the laying of tiles is completed, use cardboard and other cover brick surface, and at least 24 hours before walking on the brick surface.